Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.30 W/m-K @Temperature 100 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 80 A Dense Refractory Brick Description: A 78% alumina, bauxite based, quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from s.. |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 100 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 80 AP Dense Refractory Brick Description: This phosphate bonded bauxite brick has an improved resistance against slag attack.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.. |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 100 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 80 B Dense Refractory Brick Description: A brick made from very pure Guyana bauxite. For applications under severe working conditions such as electric arc furnace roofs.Remarks: This data represents average values, obtained fr.. |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 100 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 80 Dense Refractory Brick Description: A bauxite based quality with a high abrasion resistance. Widely used in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were cut from standa.. |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 100 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 82 A Dense Refractory Brick Description: A high alumina bauxite based quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from sa.. |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 650 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 85 K Dense Refractory Brick Description: Corundum based bricks with a mullite bond. Application: rotating incinerator furnacesRemarks: This data represents average values, obtained from samples that were cut from standard bric.. |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 650 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 85 P1 Dense Refractory Brick Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. In order to optimized the resistance against aluminum attack the sum of Al2O.. |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 650 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 90 Dense Refractory Brick Description: This brick can be used in very severe conditions, i.e. in reducing atmosphere at a high temperatures, e.g. in carbon-black furnaces.Remarks: This data represents average values, obtaine.. |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 1100 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast LP 85 AM Dense Refractory Brick Description: LP 85 AM is a brick based on bauxite with a mullite bond. It is characterized by a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, iron lad.. |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 1100 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast LP 85 M Dense Refractory Brick Description: A bauxite brick with a mullite bond with a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, outlet cement kilns, electric arc furnace roofs... |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 650 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 85 KP Dense Refractory Brick Description: This corundum based phosphate bond brick is characterized by a very low porosity, high slag resistance and high strength. Application: rotating incinerator furnaces.Remarks: This data r.. |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 650 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 85 M Dense Refractory Brick Description: A bauxite based brick with a mullite bond. Application: torpedo ladles, electric arc furnace roofs, cement kilns.Remarks: This data represents average values, obtained from samples that.. |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 650 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 85 PW Dense Refractory Brick Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. Application: aluminum holding furnaces.Remarks: This data represents average.. |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 650 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 86 A Dense Refractory Brick Description: This bauxite based brick has a high strength and good erosion resistance. Application in torpedo ladles for the steel industry and outlet zone rotary cement kilns.Remarks: This data rep.. |
|||
Thermal Conductivity | 2.30 - 2.40 W/m-K @Temperature 100 °C |
16.0 - 16.7 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 90 Moldable Refractory Material Description: This high refractory ramming material contains several well defined corundum qualities and only a small quantity of binding agent. Curas 90 has a very good resistance against erosion an.. |
|||
Thermal Conductivity | 2.31 W/m-K @Temperature 316 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 600 °F |
|
Crucible Steel CPM® Nu-Die® EZ Tool Steel CRUCIBLE CPM Nu-Die EZ is a new, patented die and mold steel designed for service as die casting dies and plastic injection molds. It is supplied in the prehardened condition, and is easily machined.. |
|||
Thermal Conductivity | 2.31 W/m-K @Temperature 316 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 600 °F |
|
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11 Halcomb 218 is a general purpose hot work tool steel, combining good toughness with moderate high-temperature strength and heat check resistance. Because of its high toughness, it is particularly su.. |
|||
Thermal Conductivity | 2.31 W/m-K @Temperature 316 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 600 °F |
|
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel Crucible PDCQ™ is a premium version of H13, manufactured to exceed die casting industry specifications. PDCQ has at least 10 ft. lbs room temperature transverse toughness. Its enhanced toughness pr.. |
|||
Thermal Conductivity | 2.30 W/m-K @Temperature 1100 °C |
16.0 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast LP 85 KP Dense Refractory Brick Description: This mullite and phosphate bonded corundum brick has a very low porosity, a high strength and a good thermal shock resistance. This quality has a very good resistance against slag. Appl.. |