Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 20.5 W/m-K @Temperature 500 °C |
142 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 500 °C |
142 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 500 °C |
142 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 500 °C |
142 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 500 °C |
142 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 500 °C |
142 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 500 °C |
142 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 600 °C |
142 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 600 °C |
142 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F) Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 700.0 °C |
142 BTU-in/hr-ft²-°F @Temperature 1292 °F |
|
AK Steel 13-4 SR® Ferritic Stainless Steel AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 20.0 °C |
142 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Assab Steels ASSAB XW-5 Cold Work Steel ASSAB XW-5 is a high-carbon, high chromium tool steel alloyed with tungsten, characterized by:High wear resistanceHigh compressive strengthHigh surface hardness after hardeningGood through-hardening.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 500 °C |
142 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 500 °C |
142 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 600 °C |
142 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 10 hours at 649°C (1200°F) Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 600 °C |
142 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Thermal Conductivity | 20.5 W/m-K @Temperature 343 °C |
142 BTU-in/hr-ft²-°F @Temperature 650 °F |
|
Schmolz + Bickenbach Cryodur® 2379 (D-2) Cold Work Die Steel Description: Cryodur® 2379 is a high carbon, high chromium tool steel developed for high wear applications and Supplied in the annealed conditionCharacteristics: Excellent abrasive wear resistance;.. |