Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.46 W/m-K @Temperature 538 °C |
10.1 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek Pyrocast ALFS Abrasion-Resistant Refractory Castable Pyrocast ALFS refractory is a high flow, fused silica castable. At low water levels (6.5-7%), Pyrocast ALFS exhibits outstanding flow characteristics.ApplicationsAluminum melting equipment Aluminum.. |
|||
Thermal Conductivity | 1.45 W/m-K @Temperature 700 °C |
10.1 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Pyrotek Pyrocast 220HT Refractory Castable Pyrocast 220HT is a high-performance refractory castable based on fused silica and silicon carbide.ApplicationsTransfer troughs Launder linings Filter boxes Pins and spouts AdvantagesThermal shock r.. |
|||
Thermal Conductivity | 1.45 W/m-K @Temperature 1100 °C |
10.1 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 42 Dense Refractory Brick Description: Because of its abrasion resistance and high density, this brick performs very well in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were c.. |
|||
Thermal Conductivity | 1.45 - 1.65 W/m-K @Temperature 100 °C |
10.1 - 11.5 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 180 B Dense Refractory Castable Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can.. |
|||
Thermal Conductivity | 1.45 - 1.65 W/m-K @Temperature 100 °C |
10.1 - 11.5 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 180 Dense Refractory Castable Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th.. |
|||
Thermal Conductivity | 1.45 - 1.65 W/m-K @Temperature 100 °C |
10.1 - 11.5 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 180 TF Dense Refractory Castable Description: Curon 180 TF is a tabular alumina based castable, highly abrasion resistant, especially developed for application in the vacuum ladle treatment installation in the steel refinery.Remark.. |
|||
Thermal Conductivity | 1.45 - 1.55 W/m-K @Temperature 1400 °C |
10.1 - 10.8 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 160 H GS (R) Dense Vibrating Refractory Castable Description: Vibron 160 H GS (R) is a pumpable low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock-, corrosion- and abrasion resista.. |
|||
Thermal Conductivity | 1.45 - 1.65 W/m-K @Temperature 600 °C |
10.1 - 11.5 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 160 H SiC Dense Vibrating Refractory Castable Description: Vibron 160 H SiC is a low cement vibrating castable characterized by a high strength, good abrasion resistance and excellent thermal shock resistance. Because of the presence of SiC, th.. |
|||
Thermal Conductivity | 1.45 - 1.65 W/m-K @Temperature 1400 °C |
10.1 - 11.5 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide.. |
|||
Thermal Conductivity | 1.45 W/m-K @Temperature 1100 °C |
10.1 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast A 1 S Dense Refractory Brick Description: A brick with a high creep resistance, successfully applied in anode baking furnaces and in the transition zone of rotary cement kilns.Remarks: This data represents average values, obtai.. |
|||
Thermal Conductivity | 1.46 W/m-K @Temperature 1100 °C |
10.1 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 44 Dense Refractory Brick Description: A very dense, high duty fireclay brick with low iron and alkali content. Widely used in anode-baking furnaces (aluminum industry) and as the lining of the top of blast furnaces.Remarks:.. |
|||
Thermal Conductivity | 1.45 W/m-K @Temperature 800 °C, Time 10800 sec |
10.1 BTU-in/hr-ft²-°F @Temperature 1470 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST A High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Thermal Conductivity | 1.45 W/m-K @Temperature 600 °C, Time 10800 sec |
10.1 BTU-in/hr-ft²-°F @Temperature 1110 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST LC70 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Thermal Conductivity | 1.45 - 1.65 W/m-K @Temperature 100 °C |
10.1 - 11.5 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply .. |
|||
Thermal Conductivity | 1.46 W/m-K @Temperature 1100 °C |
10.1 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 45 Dense Refractory Brick Description: High quality refractory brick with a good volume stability up to 1450°C. Used where high load bearing capacities are required e.g. blast furnace stoves.Remarks: This data represents av.. |