Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.178 W/m-K @Temperature 51.0 °C |
1.24 BTU-in/hr-ft²-°F @Temperature 124 °F |
ASTM C518 |
3M 941 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Thermal Conductivity | 0.178 W/m-K @Temperature 51.0 °C |
1.24 BTU-in/hr-ft²-°F @Temperature 124 °F |
ASTM C518 |
3M 9461P Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Thermal Conductivity | 0.178 W/m-K @Temperature 51.0 °C |
1.24 BTU-in/hr-ft²-°F @Temperature 124 °F |
ASTM C518 |
3M 9461PC Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Thermal Conductivity | 0.178 W/m-K @Temperature 51.0 °C |
1.24 BTU-in/hr-ft²-°F @Temperature 124 °F |
ASTM C518 |
3M 965 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Thermal Conductivity | 0.178 W/m-K @Temperature 51.0 °C |
1.24 BTU-in/hr-ft²-°F @Temperature 124 °F |
ASTM C518 |
3M 966 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Thermal Conductivity | 0.178 W/m-K @Temperature 51.0 °C |
1.24 BTU-in/hr-ft²-°F @Temperature 124 °F |
ASTM C518 |
3M 9462P Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Thermal Conductivity | 0.179 W/m-K @Temperature 177 °C |
1.24 BTU-in/hr-ft²-°F @Temperature 351 °F |
|
3M Interam™ E-5A-4 Endothermic Mat When properly installed, 3M Interam Endothermic Mat E-5A-4 provides a uniform covering that, when exposed to high temperatures, releases chemically-bound water to cool the outer surfaces of the wrap.. |