Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 32.0 W/m-K @Temperature 599 °C |
222 BTU-in/hr-ft²-°F @Temperature 1110 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM DIEVAR® Hot Work Tool Steel Description: Uddeholm Dievar is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross cracking, hot wear and plastic.. |
|||
Thermal Conductivity | 32.0 W/m-K @Temperature 20.0 °C |
222 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Assab Steels DF-3 Cold Work Steel DF-3 general purpose oil-hardening tool steel is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include:Good machinabil.. |
|||
Thermal Conductivity | 32.0 W/m-K @Temperature 600 °C |
222 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |
|||
Thermal Conductivity | 32.0 W/m-K @Temperature 400 °C |
222 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
Thermal Conductivity | 32.0 W/m-K @Temperature 343 °C |
222 BTU-in/hr-ft²-°F @Temperature 650 °F |
|
Schmolz + Bickenbach Cryodur® 2510 (O-1) Cold Work Die Steel Description: Cyrodur ® 2510 is a single melt Extra Fine Structure (EFS) material; and Supplied in the soft annealed conditionCharacteristics: Excellent dimensional stability during heat treatment; .. |
|||
Thermal Conductivity | 32.0 W/m-K @Temperature 20.0 °C |
222 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
hardened to 62 HRC |
Bohler-Uddeholm O1 Cold Work Tool Steel Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha.. |