Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 29.5 W/m-K @Temperature 199 °C |
205 BTU-in/hr-ft²-°F @Temperature 390 °F |
|
EDRO #3 Prehardened Mold Quality P20 Alloy Steel EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with.. |
|||
Thermal Conductivity | 29.5 W/m-K @Temperature 200 °C |
205 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Bohler-Uddeholm BÖHLER M261 Extra Plastic Lens Mold Steel VACUUM ARC REMELTED HARDENED AND TEMPERED PLASTIC LENS MOLD STEELBOHLER M261 follow current trends in tool and die-making:Excellent machinability coupled with higher hardnessGood dimensional stabili.. |
|||
Thermal Conductivity | 29.5 W/m-K @Temperature 199 °C |
205 BTU-in/hr-ft²-°F @Temperature 390 °F |
hardened to 310 HB |
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel Cr-Mo alloyed steelP20 Modified offers the following benefits:No hardening risksNo hardening costsTime saving, e.g. no waiting for heat treatmentLower tool cost (e.g. no distortion to rectify)Modifi.. |
|||
Thermal Conductivity | 29.5 W/m-K @Temperature 200 °C |
205 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Assab Steels 618 Plastic Mold Material ASSAB 618 is a vacuum-degassed Cr-Ni-Mo-alloy steel which is supplied in the hardened and tempered condition. ASSAB 618 is manufactured to consistently high quality standards with a controlled sulfu.. |
|||
Thermal Conductivity | 29.5 W/m-K @Temperature 200 °C |
205 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Assab Steels 718HH Plastic Mold Material IMPAX SUPREME is a premium-quality vacuum-degassed Cr-Ni-Mo-alloyed steel which is supplied in the hardened and tempered condition. IMPAX SUPREME is manufactured to consistently high quality standar.. |