Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 27.4 W/m-K @Temperature 300 °C |
190 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |
|||
Thermal Conductivity | 27.4 W/m-K @Temperature 400 °C |
190 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |