Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 26.8 W/m-K @Temperature 649 °C |
186 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
International Mold Steel Premium H13 Hot Work Die and Mold Steel Description: International Mold Steel's Premium H-13 is a chromium-based, hot work die and plastic mold steel designed for increased production rates and longer tool life. It meets the restricti.. |
|||
Thermal Conductivity | 26.8 W/m-K @Temperature 649 °C |
186 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Latrobe LSSâ„¢ H13 PQ Hot Work Tool Steel TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications... |
|||
Thermal Conductivity | 26.8 W/m-K @Temperature 649 °C |
186 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Latrobe LSSâ„¢ H13 Tool Steel (ASTM H13) TLS H13 tool steel is a versatile chromium-molybdenum hot work steel that is widely used in hot work and cold work tooling applications. The hot hardness (hot strength) of H13 resists thermal fatigu.. |
|||
Thermal Conductivity | 26.8 W/m-K @Temperature 649 °C |
186 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Latrobe Viscount 20® Free Machining Tool Steel (ASTM H13S) Viscount 20 tool steel is a resulfurized H13 tool steel. The distribution of alloy sulfide particles in the microstructure enhances the machinability of the steel in the annealed condition. In addi.. |
|||
Thermal Conductivity | 26.8 W/m-K @Temperature 150 °C |
186 BTU-in/hr-ft²-°F @Temperature 302 °F |
|
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |
|||
Thermal Conductivity | 26.8 W/m-K @Temperature 500 °C |
186 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |