Polymer Property : Thermal Conductivity = 26.2 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 26.2 W/m-K

@Temperature 1000 °C
182 BTU-in/hr-ft²-°F

@Temperature 1832 °F
AK Steel 13-4 SR® Ferritic Stainless Steel
AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w..
Thermal Conductivity 26.2 W/m-K

@Temperature 400 °C
182 BTU-in/hr-ft²-°F

@Temperature 752 °F
Assab Steels 8407 2M Hot Work Steel
ASSAB 8407 is a chromium-molybdenum-vanadium-alloyed steel which is characterized by: Good resistance to abrasion at both low and high temperatures. High level of toughness and ductility Uniform ..
Thermal Conductivity 26.2 W/m-K

@Temperature 400 °C
182 BTU-in/hr-ft²-°F

@Temperature 752 °F
Assab Steels 8407 SUPREME Hot Work Steel
8407 SUPREME is characterized by:High level of resistance to thermal shock and thermal fatigueGood high temperature strengthExcellent toughness and ductility in all directionsGood machinability and ..