Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 24.8 W/m-K @Temperature 800 °C |
172 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Thermal Conductivity | 24.8 W/m-K @Temperature 900.0 °C |
172 BTU-in/hr-ft²-°F @Temperature 1652 °F |
|
AK Steel 13-4 SR® Ferritic Stainless Steel AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w.. |
|||
Thermal Conductivity | 24.8 W/m-K @Temperature 25.0 °C |
172 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 468°C Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c.. |
|||
Thermal Conductivity | 24.8 W/m-K @Temperature 50.0 °C |
172 BTU-in/hr-ft²-°F @Temperature 122 °F |
|
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 482°C Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c.. |
|||
Thermal Conductivity | 24.8 W/m-K @Temperature 100 °C |
172 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
AK Steel 410 Cb Martensitic Stainless steel AK Steel 410 Cb is an improved version of standard Type 410. The addition of columbium offers 3 major advantages: 1) Greater ease in heat treating, 2) Higher strength and toughness, 3) Improved gra.. |