Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 23.6 W/m-K @Temperature 900 °C |
164 BTU-in/hr-ft²-°F @Temperature 1650 °F |
|
Special Metals INCONEL® alloy 693 INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t.. |