Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 21.6 W/m-K @Temperature 600 °C |
150 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 21.6 W/m-K @Temperature 600 °C |
150 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 21.6 W/m-K @Temperature 600 °C |
150 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 21.6 W/m-K @Temperature 600 °C |
150 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 21.6 W/m-K @Temperature 600 °C |
150 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 21.6 W/m-K @Temperature 600 °C |
150 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Thermal Conductivity | 21.6 W/m-K @Temperature 538 °C |
150 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Crucible Steel 303 Plus Chromium-Nickel Steel Crucible 303 Plus is a non-hardenable austenitic chromium-nickel steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of.. |
|||
Thermal Conductivity | 21.6 W/m-K @Temperature 538 °C |
150 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Crucible Steel 303 SE Chromium-Nickel Steel Crucible 303 SE is a non-hardenable austenitic chromium-nickel steel to which selenium has been added to improve machinability and non-galling characteristics. This grade is non-magnetic in the anne.. |
|||
Thermal Conductivity | 21.6 W/m-K @Temperature 538 °C |
150 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Crucible Steel 347 Chromium-Nickel Steel Crucible 347 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi.. |
|||
Thermal Conductivity | 21.6 W/m-K @Temperature 538 °C |
150 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Crucible Steel 348 Chromium-Nickel Steel Crucible 348 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi.. |
|||
Thermal Conductivity | 21.6 W/m-K @Temperature 538 °C |
150 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Crucible Steel 304L Chromium-Nickel Steel Crucible 304L is a non-hardenable, low carbon austenitic chromium-nickel steel designed for special applications. It is particularly suitable for applications requiring welding operations where it i.. |