Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 21.2 W/m-K @Temperature 540 °C |
147 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Haynes 617 Nickel Alloy Plate Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed.. |