Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, all-weld metal, GTAW weld 3.2 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, mill annealed HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GMAW spray weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 25.4 mm thick bar HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 30% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 50% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 1 hour at 500°C, air cooled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 5000 hours at 500°C, air cooled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 6.4 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 9.5 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, plate and bar HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 482 °C |
141 BTU-in/hr-ft²-°F @Temperature 900 °F |
|
Crucible Steel XM-19 Stainless Steel Crucible XM-19 Stainless is a nitrogen strengthened, low carbon, austenitic, stainless steel that provides good corrosion resistance in combination with high strength. The alloy has better corrosio.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 0.71 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 10% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW short arc weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 19.1 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 31.8 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 20.3 W/m-K @Temperature 500 °C |
141 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |