Polymer Property : Thermal Conductivity = 18.2 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 18.2 W/m-K

@Temperature 500 °C
126 BTU-in/hr-ft²-°F

@Temperature 932 °F
Annealed Condition
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel
A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re..
Thermal Conductivity 18.2 W/m-K

@Temperature 300 °C
126 BTU-in/hr-ft²-°F

@Temperature 572 °F
AK Steel 13-4 SR® Ferritic Stainless Steel
AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w..
Thermal Conductivity 18.2 W/m-K

@Temperature 400 °C
126 BTU-in/hr-ft²-°F

@Temperature 752 °F
Carpenter 20-Mo6® Stainless Steel, Plate
Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, ..
Thermal Conductivity 18.2 W/m-K

@Temperature 400 °C
126 BTU-in/hr-ft²-°F

@Temperature 752 °F
Carpenter 20-Mo6® Stainless Steel, Strip
Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, ..
Thermal Conductivity 18.2 W/m-K

@Temperature 400 °C
126 BTU-in/hr-ft²-°F

@Temperature 752 °F
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C
Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, ..
Thermal Conductivity 18.2 W/m-K

@Temperature 200 °C
126 BTU-in/hr-ft²-°F

@Temperature 392 °F
condition H 900
Carpenter Custom 450® Stainless Steel, Annealed
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Thermal Conductivity 18.2 W/m-K

@Temperature 200 °C
126 BTU-in/hr-ft²-°F

@Temperature 392 °F
condition H 900
Carpenter Custom 450® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F))
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Thermal Conductivity 18.2 W/m-K

@Temperature 200 °C
126 BTU-in/hr-ft²-°F

@Temperature 392 °F
condition H 900
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Thermal Conductivity 18.2 W/m-K

@Temperature 200 °C
126 BTU-in/hr-ft²-°F

@Temperature 392 °F
condition H 900
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Thermal Conductivity 18.2 W/m-K

@Temperature 200 °C
126 BTU-in/hr-ft²-°F

@Temperature 392 °F
condition H 900
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Thermal Conductivity 18.2 W/m-K

@Temperature 200 °C
126 BTU-in/hr-ft²-°F

@Temperature 392 °F
condition H 900
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..