Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 17.1 W/m-K @Temperature 300 °C |
119 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 17.1 W/m-K @Temperature 300 °C |
119 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 17.1 W/m-K @Temperature 300 °C |
119 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 17.1 W/m-K @Temperature 300 °C |
119 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 17.1 W/m-K @Temperature 300 °C |
119 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 17.1 W/m-K @Temperature 300 °C |
119 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 17.1 W/m-K @Temperature 300 °C |
119 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Thermal Conductivity | 17.1 W/m-K @Temperature 500 °C |
119 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Special Metals INCONEL® alloy 740 Precipitation-Hardenable Ni-Cr-Co Superalloy INCONEL® alloy 740 is a nickel-chromium-cobalt alloy developed by Special Metals Corporation. The alloy is age hardenable by the precipitation of a gamma prime second phase. Potential applicati.. |
|||
Thermal Conductivity | 17.1 W/m-K @Temperature 300 °C |
119 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Thermal Conductivity | 17.1 W/m-K @Temperature 300 °C |
119 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |