Thermal Properties Metric English Comments
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, all-weld metal, GTAW weld 3.2 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, mill annealed
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 400 °C
116 BTU-in/hr-ft²-°F

@Temperature 752 °F
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Thermal Conductivity 16.7 W/m-K

@Temperature 400 °C
116 BTU-in/hr-ft²-°F

@Temperature 752 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GMAW spray weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 25.4 mm thick bar
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 30% cold rolled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 50% cold rolled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 1 hour at 500°C, air cooled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 5000 hours at 500°C, air cooled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 6.4 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 9.5 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, plate and bar
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid..
Thermal Conductivity 16.7 W/m-K

@Temperature 20.0 °C
116 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Schmolz + Bickenbach UGIMA® 304 Cu Stainless Steel Bar
Description: 304Cu UGIMA® is an enhanced machining grade produced only by Ugitech, providing the ultimate level of machinability available in an non-resulfurized austenitic stainless steel. 304Cu..
Thermal Conductivity 16.7 W/m-K

@Temperature 400 °C
116 BTU-in/hr-ft²-°F

@Temperature 752 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 10 hours at 649°C (1200°F)
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Thermal Conductivity 16.7 W/m-K

@Temperature 400 °C
116 BTU-in/hr-ft²-°F

@Temperature 752 °F
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 0.71 mm thick sheet
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 10% cold rolled
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW short arc weld 1.1 mm diameter filler wire
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 19.1 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 31.8 mm thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Thermal Conductivity 16.7 W/m-K

@Temperature 20.0 °C
116 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Schmolz + Bickenbach Cryodur® 2379 (D-2) Cold Work Die Steel
Description: Cryodur® 2379 is a high carbon, high chromium tool steel developed for high wear applications and Supplied in the annealed conditionCharacteristics: Excellent abrasive wear resistance;..
Thermal Conductivity 16.7 W/m-K

@Temperature 300 °C
116 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate
HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin..
Copyright © lookpolymers.com All Rights Reserved