Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 14.0 W/m-K @Temperature 200 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 200 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 200 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 200 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 200 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 200 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 200 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 200 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged 16000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 200 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® S alloy, weld metal, aged at 649°C (1200°F) for 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 200 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 200 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 1000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 200 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications .. |
|||
Thermal Conductivity | 14.0 W/m-K @Temperature 200 °C |
97.2 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |