Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, all-weld metal, GTAW weld 3.2 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, mill annealed HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 200 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 200 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GMAW spray weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld 3.2 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 25.4 mm thick bar HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 30% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 50% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 1 hour at 500°C, air cooled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 5000 hours at 500°C, air cooled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 6.4 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 9.5 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, all-weld metal, GMAW weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, plate and bar HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 200 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 200 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 200 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 0.71 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 10% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW short arc weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 19.1 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 31.8 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 200 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 200 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Thermal Conductivity | 11.9 W/m-K @Temperature 100 °C |
82.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |