Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.80 W/m-K @Temperature 1100 °C |
12.5 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 60 M Dense Refractory Brick Description: This quality is produced from high fired raw materials with a high mullite content. The grain distribution for these bricks is carefully selected, so that a maximum density is obtained... |
|||
Thermal Conductivity | 1.80 W/m-K @Temperature 400 °C, Time 10800 sec |
12.5 BTU-in/hr-ft²-°F @Temperature 752 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST LC70 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Thermal Conductivity | 1.80 W/m-K @Temperature 100 °C |
12.5 BTU-in/hr-ft²-°F @Temperature 212 °F |
Thru-thickness |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.80 W/m-K @Temperature 200 °C |
12.5 BTU-in/hr-ft²-°F @Temperature 392 °F |
Thru-thickness |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.80 W/m-K @Temperature 300 °C |
12.5 BTU-in/hr-ft²-°F @Temperature 572 °F |
Thru-thickness |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.80 W/m-K @Temperature 500 °C |
12.5 BTU-in/hr-ft²-°F @Temperature 932 °F |
Thru-thickness |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 1.80 - 2.20 W/m-K @Temperature 100 °C |
12.5 - 15.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 180 Refractory Insulating Castable Description: Hollow alumina spheres are used as an aggregate for this castable. With very low percentages of Fe2O3 and SiO2, it is well resistant against reducing and corrosive kiln atmospheres.Rema.. |