Polymer Property : Thermal Conductivity = 1.41 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.41 W/m-K

@Temperature 650 °C
9.79 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast AK 53 E Dense Refractory Brick
Description: Because of its very high erosion resistance this brick is applied in e.g. recirculation cyclones for CFB coal fired boilers.Remarks: This data represents average values, obtained from s..
Thermal Conductivity 1.41 - 1.42 W/m-K

@Temperature 1600 °C
9.79 - 9.85 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Gouda Vuurvast CURON 180 T SP GM Dense Refractory Castable
Description: Curon 180 T SP GM is a gunning castable based on tabular alumina for application at very high temperatures.Remarks: These values apply to cast products.Information provided by Gouda Vuu..