Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.25 W/m-K @Temperature 650 °C |
8.68 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast A Vuurvast Dense Refractory Brick Description: A general purpose high quality fireclay brick for use up to 1400°C. Reasonably good thermal shock resistance.Remarks: This data represents average values, obtained from samples that .. |
|||
Thermal Conductivity | 1.25 W/m-K @Temperature 650 °C |
8.68 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast B 1 Sp Dense Refractory Brick Description: High mechanical strength and very low porosity are typical for this type of brick. Application: transition zone in cement kilns, incinerators, steel ladles.Remarks: This data represents.. |
|||
Thermal Conductivity | 1.25 - 1.45 W/m-K @Temperature 100 °C |
8.68 - 10.1 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 90 PF Moldable Refractory Material Description: Curas 90 PF ramming mix with outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). The product is supplied in two components: a dry powder and a liquid. Curas 90 PF i.. |
|||
Thermal Conductivity | 1.25 - 1.45 W/m-K @Temperature 100 °C |
8.68 - 10.1 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 90 PF REPAIR Moldable Refractory Material Description: Curas 90 PF Repair ramming mix is especially developed for repairing purposes of Curas 90 PF linings. The product is supplied in two components: a dry powder and a liquid. Detailed inst.. |
|||
Thermal Conductivity | 1.25 - 1.45 W/m-K @Temperature 100 °C |
8.68 - 10.1 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS 90 PFM Moldable Refractory Material Description: Curas 90 PFM ramming mix has outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). In addition, it has a good resistance against thermal shock and corrosive gasses. T.. |
|||
Thermal Conductivity | 1.25 - 1.45 W/m-K @Temperature 600 °C |
8.68 - 10.1 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 180 T SP GM Dense Refractory Castable Description: Curon 180 T SP GM is a gunning castable based on tabular alumina for application at very high temperatures.Remarks: These values apply to cast products.Information provided by Gouda Vuu.. |
|||
Thermal Conductivity | 1.25 - 1.35 W/m-K @Temperature 100 °C |
8.68 - 9.37 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 170 M Dense Vibrating Refractory Castable Description: Vibron 170 is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid slags.Remar.. |
|||
Thermal Conductivity | 1.25 - 1.35 W/m-K @Temperature 100 °C |
8.68 - 9.37 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 170 M GS (R) Dense Vibrating Refractory Castable Description: Vibron 170 M GS (R) is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sl.. |
|||
Thermal Conductivity | 1.25 W/m-K @Temperature 100 °C |
8.68 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 44 Dense Refractory Brick Description: A very dense, high duty fireclay brick with low iron and alkali content. Widely used in anode-baking furnaces (aluminum industry) and as the lining of the top of blast furnaces.Remarks:.. |
|||
Thermal Conductivity | 1.25 - 1.35 W/m-K @Temperature 100 °C |
8.68 - 9.37 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 170 M RAPID Dense Vibrating Refractory Castable Description: Vibron 170 M Rapid is a low cement castable based on synthetic mullite grog and is characterized by a high strength, excellent thermal shock resistance and high resistance to liquid sla.. |
|||
Thermal Conductivity | 1.25 W/m-K @Temperature 600.0 °C |
8.67 BTU-in/hr-ft²-°F @Temperature 1112 °F |
|
Stellar Canada CERAMITE® SFR Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |
|||
Thermal Conductivity | 1.25 W/m-K @Temperature 100 °C |
8.68 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 45 Dense Refractory Brick Description: High quality refractory brick with a good volume stability up to 1450°C. Used where high load bearing capacities are required e.g. blast furnace stoves.Remarks: This data represents av.. |
|||
Thermal Conductivity | 1.25 - 1.45 W/m-K @Temperature 1000 °C |
8.68 - 10.1 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast FLUCON 160 H Dense Self Flowing Refractory Castable Description: Flucon 160 H is a self-flowing low cement castable on high fired high alumina grog base, characterized by a high strength and good thermal shock resistance.Remarks: These values apply t.. |