Polymer Property : Thermal Conductivity = 0.820 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.820 W/m-K

@Temperature 700 °C
5.69 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Pyrotek Pyrocast AR Castable Refractory
Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyro..
Thermal Conductivity 0.820 W/m-K

@Temperature 700 °C
5.69 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Pyrotek Pyrocast AR FINE Castable Refractory
Pyrocast AR Fine is a fine-grain fused silica castable, offering similar insulation properties, yet lighter weight that the Pyrocast AR formulation. Pyrocast AR Fine is suited for thin wall casting..
Thermal Conductivity 0.820 W/m-K

@Temperature 815 °C
5.69 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Pyrotek Pyrocast ICL Castable Refractory
Pyrocast ICL was developed exclusively for the induction furnace market as a coil lining refractory. This silica and alumina based material displays high strength and excellent thermal shock resist..
Thermal Conductivity 0.820 - 0.920 W/m-K

@Temperature 600 °C
5.69 - 6.38 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 150 RN Dense Refractory Castable
Description: This on sintered bauxite and low-iron alumina cement based castable contains stainless steel fibers, what results in a very good mechanical strength.Remarks: These values apply to cast ..
Thermal Conductivity 0.820 - 0.920 W/m-K

@Temperature 600 °C
5.69 - 6.38 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 160 C Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 C has an excellent thermal shoc..
Thermal Conductivity 0.820 - 0.920 W/m-K

@Temperature 1400 °C
5.69 - 6.38 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Gouda Vuurvast CURON 160 HS GM Dense Refractory Castable
Description: This gunning castable has a high volume stability up to high temperatures. In addition Curon 160 HS GM has an excellent thermal shock resistance and abrasion resistance (9-12 cm3 accord..
Thermal Conductivity 0.820 - 0.920 W/m-K

@Temperature 600 °C
5.69 - 6.38 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 150 Dense Refractory Castable
Description: This bauxite based castable has a very good thermal shock resistance and is therefore well suited for burner blocks.Remarks: These values apply to cast products. Also available in gunni..