Polymer Property : Thermal Conductivity = 0.560 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.560 - 0.660 W/m-K

@Temperature 1000 °C
3.89 - 4.58 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 120 C Dense Refractory Castable
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 C has good thermal shock resistance.Remarks: These values apply to cast products.Informat..
Thermal Conductivity 0.560 - 0.660 W/m-K

@Temperature 600 °C
3.89 - 4.58 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 130 Dense Refractory Castable
Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap..
Thermal Conductivity 0.560 - 0.660 W/m-K

@Temperature 600 °C
3.89 - 4.58 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 140 Dense Refractory Castable
Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo..
Thermal Conductivity 0.560 - 0.660 W/m-K

@Temperature 100 °C
3.89 - 4.58 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 150 AC Dense Refractory Castable
Description: Curon 150 AC is a coarse castable for use up to 1500°C with a high strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.560 W/m-K

@Temperature 260 °C
3.89 BTU-in/hr-ft²-°F

@Temperature 500 °F
ASTM C182
BNZ Materials BNZ-32 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..