Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.490 - 0.590 W/m-K @Temperature 600 °C |
3.40 - 4.09 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 110 C Dense Refractory Castable Description: Curon 110 C is a coarse castable. Application: covers for anode baking furnaces.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.490 - 0.590 W/m-K @Temperature 600 °C |
3.40 - 4.09 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 110 Dense Refractory Castable Description: Curon 110 is an easily workable castable, especially developed to cast complicated shapes. Because of its low shrinkage, this castable has less tendency to crack.Remarks: These values a.. |
|||
Thermal Conductivity | 0.490 - 0.590 W/m-K @Temperature 600 °C |
3.40 - 4.09 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 145 P Dense Refractory Castable Description: This material with an extreme plasticity is well suited for repair work or application as a thin layer.Remarks: These values apply to cast products.Information provided by Gouda Vuurvas.. |
|||
Thermal Conductivity | 0.490 - 0.590 W/m-K @Temperature 100 °C |
3.40 - 4.09 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 150 HS GM Dense Refractory Castable Description: Curon 150 HS GM is an abrasion resistant gunning castable for use up to 1500°C.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.490 - 0.690 W/m-K @Temperature 200 °C |
3.40 - 4.79 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Gouda Vuurvast FI 65-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.490 - 0.690 W/m-K @Temperature 600 °C |
3.40 - 4.79 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast FI 65-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.490 - 0.590 W/m-K @Temperature 600 °C |
3.40 - 4.09 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 100 C Dense Refractory Castable Description: Curon 100 C can be applied up to 1000°C, under normal operating conditions and is especially applied in the bottom of electrolytic cells in the aluminum industry.Remarks: These values .. |