Polymer Property : Thermal Conductivity = 0.460 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.460 W/m-K

@Temperature 607 °C
3.19 BTU-in/hr-ft²-°F

@Temperature 1120 °F
hot face 744°C, cold face 470°C, mean - 607°C
Pyrotek Insural® 140 Insulating Refractory Shapes for Aluminum
Insural® 140 Precast Shapes are designed for the containment of molten aluminum in hot top modules (cross feeder) and trough/launder applications.AdvantagesNear zero expansion avoids gaps at the jo..
Thermal Conductivity 0.460 - 0.560 W/m-K

@Temperature 1370 °C
3.19 - 3.89 BTU-in/hr-ft²-°F

@Temperature 2500 °F
Gouda Vuurvast GOLITE 140 Refractory Insulating Castable
Description: This castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere.Remarks:..
Thermal Conductivity 0.460 - 0.560 W/m-K

@Temperature 1370 °C
3.19 - 3.89 BTU-in/hr-ft²-°F

@Temperature 2500 °F
Gouda Vuurvast GOLITE 140 GM Refractory Insulating Castable
Description: This gunning castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere...