Thermal Properties Metric English Comments
Thermal Conductivity 0.349 W/m-K

@Temperature 260 °C
2.42 BTU-in/hr-ft²-°F

@Temperature 500 °F
Chosun Refractories DC-2BS Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity 0.349 W/m-K

@Temperature 260 °C
2.42 BTU-in/hr-ft²-°F

@Temperature 500 °F
Chosun Refractories GUN-120L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity 0.349 - 0.6979 W/m-K

@Temperature 800 °C
2.42 - 4.836 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Chosun Refractories MIX-1(1:4) Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).