Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
Pearl Engineering PEPLPET B-105C PET Bottle Grade A co-polymer used for soft drinks and other applications. |
|||
Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
Pearl Engineering PEPLPET B-109JS PET Sheet Grade Used mainly for 5 to 20 liter mineral water containers |
|||
Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
Pearl Engineering PEPLPET B-113C PET Sheet Grade Used mainly for box strapping. |
|||
Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
Pearl Engineering PEPLPET D-101-SH Monofilament Resin Used in the paper industry as paper pulp nets. |
|||
Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
Pearl Engineering PEPLPET F096H Film Grade Resin Used mainly as PET films/ sheets, known as Superbright |
|||
Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
Pearl Engineering PEPLPET F096HA Film Grade Resin Used mainly as PET films/ sheets, known as bright with anti-blocking agent. |
|||
Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
Pearl Engineering PEPLPET F097H Film Grade Resin Used mainly as PET films/ sheets, known as Superbright |
|||
Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
Pearl Engineering PEPLPET F097HA Film Grade Resin Used mainly as PET films/ sheets, known as bright with anti-blocking agent. |
|||
Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
Pearl Engineering PEPLPET FR-101-H Monofilament Resin Used as textile grade flame retardant for furniture, car and plane upholstery. |
|||
Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
Pearl Engineering PEPLPET B-07C PET Bottle Grade A co-polymer used mostly for containers. |
|||
Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
Pearl Engineering PEPLPET B-101C PET Sheet Grade A sheet grade polymer used in thick films. |
|||
Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
Pearl Engineering PEPLPET B101H Monofilament Resin Generally used in monofilament v-belts, zips and other technical applications. |
|||
Thermal Conductivity | 0.213 W/m-K @Temperature 280 °C |
1.48 BTU-in/hr-ft²-°F @Temperature 536 °F |
liquid |
Pearl Engineering PEPLPET B-103C PET Bottle Grade A co-polymer used for mineral water bottles |