Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.132 W/m-K @Temperature 200 °C |
0.916 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group Moler POROS Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Thermal Conductivity | 0.132 W/m-K @Temperature 50.0 °C |
0.913 BTU-in/hr-ft²-°F @Temperature 122 °F |
|
ChevronTexaco Texatherm® Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging .. |
|||
Thermal Conductivity | 0.132 W/m-K @Temperature 40.0 °C |
0.918 BTU-in/hr-ft²-°F @Temperature 104 °F |
|
ChevronTexaco Texatherm® Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging .. |