| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYasa 1614F UV-resistant ASA Information provided by Polykemi AB |
|||
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYasa 2008F UV-stabilized, High Flow ASA Information provided by Polykemi AB |
|||
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYasa 2410F High Flow ASA Information provided by Polykemi AB |
|||
| Vicat Softening Point | 103 °C @Load 5.001 kg |
217 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYblend 45FS GKF2505 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 103 °C @Load 5.001 kg |
217 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYabs F00 GF15 ABS, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.20 lb |
120°C/min; ASTM D1525 |
| Kingfa FW-620 Flame Retardant ABS Features:UL 94 V-0 @ 1.5-3.0mmWeather resistanceHeat resistanceGood surfaceApplications:Injection moldingOA deviceChargerTransformerInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.20 lb |
120°C/min; ASTM D1525 |
| Kingfa HC-110 Modified ABS Features:UL94 HB @ 1.6-3.0mmElectro-platingApplications:Electro-plating partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
| Vicat Softening Point | 103 °C @Load 5.00 kg |
217 °F @Load 11.0 lb |
50°C/min; ASTM D1525 |
| Kingfa HR-527A Modified ABS Features:UL94 HB @ 1.5-3.2mmHeat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
| Vicat Softening Point | 103 °C @Load 1.02 kg |
217 °F @Load 2.25 lb |
50°C/h; ISO 306 |
| Styrolution Terluran® GP-25 ABS Terluran GP-25 is an easy-flow, general purpose injection molding grade with high resistance to impact and heat distortion; intended for a wide range of applications, particularly in the housings se.. |
|||
| Vicat Softening Point | 103 °C @Load 1.02 kg |
217 °F @Load 2.25 lb |
50°C per hour; ISO 306A50 |
| Total Polystyrene Impact 3450 Aesthetic, High Fluidity, High Heat Resistance, High Impact Polystyrene POLYSTYRENE IMPACT 3450 is a high impact polystyrene with high heat resistance, good flow, high stiffness and good aesthetics. With such an ideal balance of properties, POLYSTYRENE IMPACT 3450 is w.. |
|||
| Vicat Softening Point | 103 °C @Load 0.999 kg |
217 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 1030 V0/F Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high melt flow rate, good impact resistance, high gloss, good light resistance, excellent processabilityInformation provided by Co.. |
|||
| Vicat Softening Point | 103 °C @Load 0.999 kg |
217 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 1050 AS Acrylonitrile Butadiene Styrene General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 103 °C @Load 5.10 kg |
217 °F @Load 11.2 lb |
120°C/h; ISO 306 |
| Covestro Bayblend® FR3009 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
| Vicat Softening Point | 103 °C @Load 5.00 kg |
217 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Kibisan® PN-106 L150 SAN High Clarity |
|||
| Vicat Softening Point | 103 °C @Load 5.00 kg |
217 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Kibisan® PN-107 L125 SAN High Clarity |
|||
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-709 ABS Super impact |
|||
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-716 ABS - High Flow High flow, medium impact |
|||
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-717C ABS Medium impact |
|||
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-726 ABS Electro-plating |
|||
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-726 ABS Electro-plating |
|||
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-746 ABS - High Flow High flow, medium impact |
|||
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-747 ABS High impact |
|||
| Vicat Softening Point | 103 °C @Load 5.00 kg |
217 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polyrex® PG-383 Polystyrene High heat; high strength |
|||
| Vicat Softening Point | 103 °C @Load 5.00 kg |
217 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTASAN SAN 0840 GF Styrene Acrylonitrile SAN with 20% glass fiber reinforcementExcellent dimensional stability, good heat resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-747S ABS - Extrusion High Impact Extrusion |
|||
| Vicat Softening Point | 103 °C @Load 1.00 kg |
217 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-763 ABS - Flame Retardant F.R. High Heat Weather Resistant |
|||