| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 94.0 °C @Load 5.001 kg |
201 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYasa 2410F High Flow ASA Information provided by Polykemi AB |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/hour; ISO 306 |
| Ineos ABS Lustran® 288 ABS, Injection Molding Grade Lustran® ABS 288 is a very high-flow injection molding grade of ABS (acrylonitrile butadiene styrene) with good impact strength and high gloss. It is intended for use in a wide range of applicati.. |
|||
| Vicat Softening Point | 94.1 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/hour; ISO 306 |
| Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
| Vicat Softening Point | 94.0 °C @Load 1.02 kg |
201 °F @Load 2.25 lb |
50°C/h; ISO 306 |
| Styrolution PS 456EB HIPS Styrolution PS 456EB is a high flow, high impact polystyrene with a good heat resistance and a high stiffness, developed for injection blow molding applications, especially for bottle of yot.High fl.. |
|||
| Vicat Softening Point | 94.0 °C @Load 5.10 kg |
201 °F @Load 11.2 lb |
ISO 527-2 |
| Borealis Borcom™ WG140AI Polypropylene Borcom™ WG140AI is a polypropylene microcomposite intended for injection molding. This material has an excellent balance between impact strength and stiffness, high melt flow rate and gives a good.. |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTABLEND 4500 V0 HF Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, excellent mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 1050 AS Acrylonitrile Butadiene Styrene General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 1218 V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearance, good thermal resistanceInformation provided by Cossa Po.. |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTADIENE 1640 AS Acrylonitrile Butadiene Styrene General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 94.0 °C @Load 1.00 kg |
201 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Kibiton® PB-5910 SBC High transparency, medium stiffness, toughness |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-709 ABS Super impact |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-716 ABS - High Flow High flow, medium impact |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-726 ABS Electro-plating |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-737 ABS - High Flow High flow, medium impact |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-746 ABS - High Flow High flow, medium impact |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-747 ABS High impact |
|||
| Vicat Softening Point | 94.0 °C @Load 1.00 kg |
201 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polyrex® PH-55Y Polystyrene - Food Medium impact |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
| Chi Mei Polylac® PA-746H ABS - High Flow Super high flow, medium impact |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polylac® PA-758R ABS - Transparent Transparent, Chemical Resistant |
|||
| Vicat Softening Point | 94.0 °C @Load 1.00 kg |
201 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
| Chi Mei Polyrex® PG-33 Polystyrene Standard grade |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Polyrex® PG-80 Polystyrene High strength |
|||