| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 143 °C @Load 1.00 kg |
289 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PP CIQ15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 143 °C @Load 5.001 kg |
289 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPH GF5030 HC Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 143 °C @Load 1.00 kg |
289 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PP EIP8020F Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 143 °C @Load 5.001 kg |
289 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPH GF8030 HC Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 143 °C @Load 1.00 kg |
289 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB SCANTEC PC S90R Polycarbonate Information provided by Polykemi AB |
|||
| Vicat Softening Point | 143 °C @Load 1.02 kg |
289 °F @Load 2.25 lb |
ISO 306 |
| Borealis Daplen™ EE065AI Polypropylene Elastomer Modified Daplen™ EE065AI is an elastomer modified polypropylene with increased crystallinity. This material has an excellent balance between impact strength and stiffness. The product is available in natu.. |
|||
| Vicat Softening Point | 143 °C @Load 5.10 kg |
289 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
| Vicat Softening Point | 143 °C @Load 5.10 kg |
289 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
| Vicat Softening Point | 143 °C @Load 5.10 kg |
289 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Covestro Makrolon® 2405 MAS057 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
| Vicat Softening Point | 143 °C @Load 5.10 kg |
289 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Covestro Makrolon® 2407 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng.. |
|||
| Vicat Softening Point | 143 °C @Load 5.10 kg |
289 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
| Vicat Softening Point | 143 °C @Load 5.10 kg |
289 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
| Vicat Softening Point | 143 °C @Load 5.10 kg |
289 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Covestro Makrolon® 2607 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
| Vicat Softening Point | 143 °C @Load 5.10 kg |
289 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Covestro Makrolon® 2665 MAS071 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
| Vicat Softening Point | 143 °C @Load 5.10 kg |
289 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Covestro Makrolon® 2665 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy.. |
|||
| Vicat Softening Point | 143 °C @Load 5.10 kg |
289 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Covestro Makrolon® 2667 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
| Vicat Softening Point | 143 °C @Load 5.00 kg |
289 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Wonderlite® PC-108U Polycarbonate - UV Stabilized UV Stabilized |
|||
| Vicat Softening Point | 143 °C @Load 5.00 kg |
289 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Wonderlite® PC-110L Polycarbonate - UV Stabilized Head Lamp |
|||
| Vicat Softening Point | 143 °C @Load 5.00 kg |
289 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Wonderlite® PC-110U Polycarbonate - UV Stabilized UV Stabilized |
|||
| Vicat Softening Point | 143 °C @Load 5.00 kg |
289 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Wonderlite® PC-122U Polycarbonate - UV Stabilized UV Stabilized |
|||
| Vicat Softening Point | 143 °C @Load 5.00 kg |
289 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
| Chi Mei Wonderlite® PC-110N Polycarbonate - Flame Retardant Opaque |
|||
| Vicat Softening Point | 143 °C @Load 5.10 kg |
289 °F @Load 11.2 lb |
50°C/h; ISO 306 |
| Covestro Makrolon® LQ2647 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g.. |
|||
| Vicat Softening Point | 143 °C @Load 1.00 kg |
289 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPHC K9030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 143 °C @Load 1.00 kg |
289 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPHC TS20040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||