Polymer Property : Vicat Softening Point = 311 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
ISO 527-2
Borealis Borcom™ WG140AI Polypropylene
Borcom™ WG140AI is a polypropylene microcomposite intended for injection molding. This material has an excellent balance between impact strength and stiffness, high melt flow rate and gives a good..
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
ISO 306
Borealis MG302Al Polypropylene Compound, Mineral Filled
MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt ..
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
ISO 306
Borealis PS65C40 Polypropylene Compound, Mineral Filled
PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and..
Vicat Softening Point 155 °C

@Load 0.999 kg
311 °F

@Load 2.20 lb
120°C/min; ASTM D1525/A, ISO 306/A
EPICHEM Epilon G2-PC 10% GF Polycarbonate, 10% Glass Fiber
Characteristics: 10% glass fibre filled, good mechanical properties
Vicat Softening Point 155 °C

@Load 0.999 kg
311 °F

@Load 2.20 lb
120°C/min; ASTM D1525/A, ISO 306/A
EPICHEM Epilon G4-PC 20% GF Polycarbonate, 20% Glass Fiber
Characteristics: 20% glass fibre filled, excellent mechanical properties
Vicat Softening Point 155 °C

@Load 1.00 kg
311 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH BF405510 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant
Information provided by Polykemi AB
Vicat Softening Point 155 °C

@Load 1.02 kg
311 °F

@Load 2.25 lb
ISO 306
Borealis MB350WG Polypropylene Compound, Mineral Filled
MB350WG is a 30% mineral filled polypropylene compound intended for injection molding. This material has a very high impact strength while maintaining good stiffness and is easy to process. Applic..