Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 142 °C @Load 1.00 kg |
288 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP CIQ10015ER UV Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 142 °C @Load 1.00 kg |
288 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC T20040 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 142 °C @Load 1.00 kg |
288 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPC TS4030 H Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 142 °C @Load 5.001 kg |
288 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF3050 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Vicat Softening Point | 142 °C @Load 5.001 kg |
288 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH GF5020 HC Polypropylene Homopolymer, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 142 °C @Load 1.00 kg |
288 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC TS25020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 142 °C @Load 5.001 kg |
288 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANTEC PC S60R Polycarbonate Information provided by Polykemi AB |
|||
Vicat Softening Point | 142 °C @Load 5.00 kg |
288 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Wonderloy® PC-175D PC/ABS Alloy
(discontinued **) Optical Disk |
|||
Vicat Softening Point | 142 °C @Load 0.999 kg |
288 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND 0840 GF Polycarbonate ABS Blend, 20% Glass Filled Polycarbonate and Acrylonitrile Butadiene Styrene blend with 20% glass fiber reinforcementHigh dimensional stability, high stiffnessInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 142 °C @Load 0.999 kg |
288 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND 8500 Polycarbonate ABS Blend Polycarbonate and Acrylonitrile Butadiene Styrene blendHigh thermal resistance, high impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 142 °C @Load 5.10 kg |
288 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makrolon® Rx1851 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low.. |
|||
Vicat Softening Point | 142 °C @Load 1.00 kg |
288 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC K8030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 142 °C @Load 1.00 kg |
288 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPHC TS15020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |