Thermal Properties Metric English Comments
Vicat Softening Point 122 °C

@Load 5.001 kg
252 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB SCANBLEND FS8 FR UV PC/ASA, Flame Retardant, UV-Stabilized
Information provided by Polykemi AB
Vicat Softening Point 122 °C

@Load 1.02 kg
252 °F

@Load 2.25 lb
ISO 306
Borealis Daplen™ EE255AE Polypropylene TPO Compound
Daplen™ EE255AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give..
Vicat Softening Point 122 °C

@Load 1.02 kg
252 °F

@Load 2.25 lb
ISO 306
Borealis Daplen™ EH104AE Polypropylene TPO Compound
Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high..
Vicat Softening Point 122 °C

@Load 5.10 kg
252 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® ET3036 FR PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Extru..