Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 108 °C @Load 1.00 kg |
226 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYblend 45FS GK25 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 108 °C @Load 5.001 kg |
226 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYsan FL100 F35 SAN, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 108 °C @Load 1.00 kg |
226 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs F00 GF15 ABS, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 108 °C @Load 5.001 kg |
226 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs H00 HF ABS, Heat Resistant, High Flow Information provided by Polykemi AB |
|||
Vicat Softening Point | 108 °C @Load 5.001 kg |
226 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs HF0 ABS Information provided by Polykemi AB |
|||
Vicat Softening Point | 108 °C @Load 5.001 kg |
226 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYlux 3809S PC/PBT-Blend Information provided by Polykemi AB |
|||
Vicat Softening Point | 108 °C @Load 5.001 kg |
226 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYlux 3809SLB PC/PBT-Blend, Paintable Information provided by Polykemi AB |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 168N GPPS Styrolution PS 168N is a high molecular weight, heat resistant grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. Also use as a blend componen.. |
|||
Vicat Softening Point | 108 °C @Load 1.02 kg |
226 °F @Load 2.25 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 158 N/L GPPS Styrolution PS 158N/L is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact polystyrene in heat contact applications; for.. |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 158K GPPS Styrolution PS 158K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact Styrolution PS in heat contact applications; fo.. |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution Terblend® N NG-02 UV ABS / PA, 8% Glass filled Terblend N NG-02 UV is an 8% glass fiber reinforced (UV stabilized) ABS/PA blend with enhanced dimensional stability and rigidity.High dimensional stabilityEnhanced rigidityEnhanced softening temper.. |
|||
Vicat Softening Point | 108 °C @Load 5.00 kg |
226 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 0820 HT Acrylonitrile Butadiene Styrene ABS with high thermal resistanceGood impact resistance, stiffness, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 108 °C @Load 5.00 kg |
226 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 0835 GF Acrylonitrile Butadiene Styrene, 17% Glass Filled ABS with 17% glass fiber reinforcementGood thermal resistance, good dimensional stability, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 108 °C @Load 1.02 kg |
226 °F @Load 2.25 lb |
120°C/hr; ASTM D 1525 |
Cossa Polimeri ESTALUX 9202 A Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 108 °C @Load 1.02 kg |
226 °F @Load 2.25 lb |
120°C/hr; ASTM D 1525 |
Cossa Polimeri ESTALUX 9202 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information.. |
|||
Vicat Softening Point | 108 °C @Load 0.999 kg |
226 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTASAN SAN 2000 Styrene Acrylonitrile General purpose SANGood chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 108 °C @Load 0.999 kg |
226 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTASAN SAN 3000 Styrene Acrylonitrile High melt flow rate, good chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® ET3032 FR Rubber Modified PC Blend, 10% Mineral Filled Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend.. |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® FR3006 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® FR3010 HF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® FR3010 IF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® FR3040 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Bayblend® FR3100 TV PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Bayblend® FR3110 TV PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Vicat Softening Point | 108 °C @Load 1.00 kg |
226 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Kibilac® PW-997S ASA Polymer Extrusion |
|||
Vicat Softening Point | 108 °C @Load 1.00 kg |
226 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Kibisan® PN-107 L125 SAN High Clarity |
|||
Vicat Softening Point | 108 °C @Load 1.00 kg |
226 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-747R ABS - Extrusion Attach case and refrigerator |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® FR410 MT Rubber Modified PC Blend, 10% Mineral Filled Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend.. |
|||
Vicat Softening Point | 108 °C @Load 5.10 kg |
226 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® FR630 GR PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Vicat Softening Point | 108 °C @Load 1.00 kg |
226 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-747F ABS - Extrusion Refrigerator |