Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs S20 ABS Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs SS0 GK10 ABS, High Flow Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 5.001 kg |
221 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYblend 45FS GKF2010 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 5.001 kg |
221 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANLON A 5005 PA/ABS-Blend Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 5.001 kg |
221 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANLON A 5005B PA/ABS-Blend Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 5.001 kg |
221 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANLON A 5005B UV PA/ABS-Blend Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs F00 ABS Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/min; ASTM D1525 |
Kingfa HR-527 Modified ABS Features:UL94 HB @ 1.5-3.2mmImpact resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Vicat Softening Point | 105 °C @Load 1.02 kg |
221 °F @Load 2.25 lb |
50°C/h; ISO 306 |
Styrolution Luran® S 767KE ASA Luran S 767KE is particular suitable for co-extrusion with PVC at low temperature. Hereby, it provides a glossy surface finish.Enhanced flowabilitySuitable for co-extrusion with PVCEnables high glos.. |
|||
Vicat Softening Point | 105 °C @Load 5.10 kg |
221 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution Terblend® N 3154 ASA / PA, 8% Mineral filled Terblend N 3154 is an 8% mineral filled ABS/PA blend with good dimensional stability and enhanced rigidity.High dimensional stabilityEnhanced rigidityMineral filled (8%)Information provided by Styro.. |
|||
Vicat Softening Point | 105 °C @Load 1.02 kg |
221 °F @Load 2.25 lb |
50°C/h; ISO 306 |
Styrolution Terlux® HD 2822 MABS Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well .. |
|||
Vicat Softening Point | 105 °C @Load 5.10 kg |
221 °F @Load 11.2 lb |
ISO 306 |
Borealis PS65C40 Polypropylene Compound, Mineral Filled PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and.. |
|||
Vicat Softening Point | 105 °C @Load 0.999 kg |
221 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTABLEND 4500 V0 HF Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, excellent mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 105 °C @Load 5.00 kg |
221 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 0417 GIF Acrylonitrile Butadiene Styrene, 17% Glass Filled ABS with 17% glass fiber reinforcementGood thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 105 °C @Load 5.00 kg |
221 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 3510 HT Acrylonitrile Butadiene Styrene ABS with very high impact resistanceHigh impact resistance at low temperature, high heat resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Kibilac® PW-957 ASA Polymer Injection |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Kibilac® PW-997S ASA Polymer Extrusion |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Kibisan® PN-106 L150 SAN High Clarity |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Kibisan® PN-107 L125 SAN High Clarity |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-717C ABS Medium impact |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polyrex® PH-888G Polystyrene - High gloss High impact; high gloss |
|||
Vicat Softening Point | 105 - 110 °C @Load 5.00 kg |
221 - 230 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
EPICHEM Epilac T ABS Acrylonitrile Butadiene Styrene |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-727 ABS Electro-plating |
|||
Vicat Softening Point | 105 °C @Load 5.00 kg |
221 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-747F ABS - Extrusion Refrigerator |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-757 ABS High gloss, medium impact |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-758R ABS - Transparent Transparent, Chemical Resistant |
|||
Vicat Softening Point | 105 °C @Load 5.00 kg |
221 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Polylac® PA-777B ABS - High Heat High Heat Impact |
|||
Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-763A ABS - Flame Retardant F.R. High Heat |
|||
Vicat Softening Point | 105 °C @Load 5.001 kg |
221 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs F00 GF17 ABS, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 105 °C @Load 5.10 kg |
221 °F @Load 11.2 lb |
50°C/hour; ISO 306 |
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (DAM), Injection Molding Grade Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage. |