Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 95.0 °C @Load 5.001 kg |
203 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs S20 ABS Information provided by Polykemi AB |
|||
Vicat Softening Point | 95.0 °C @Load 5.001 kg |
203 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYasa 2008F UV-stabilized, High Flow ASA Information provided by Polykemi AB |
|||
Vicat Softening Point | 95.0 °C @Load 5.00 kg |
203 °F @Load 11.0 lb |
50°C/min; ASTM D1525 |
Kingfa HC-110 Modified ABS Features:UL94 HB @ 1.6-3.0mmElectro-platingApplications:Electro-plating partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Vicat Softening Point | 95.0 °C @Load 1.00 kg |
203 °F @Load 2.20 lb |
120°C/min; ASTM D1525 |
Kingfa HF-618 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Vicat Softening Point | 95.0 °C @Load 5.10 kg |
203 °F @Load 11.2 lb |
50°C/hour; ISO 306 |
Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
Vicat Softening Point | 95.0 °C @Load 5.10 kg |
203 °F @Load 11.2 lb |
50°C/hour; ISO 306 |
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (Conditioned), Injection Molding Grade Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage. |
|||
Vicat Softening Point | 95.0 °C @Load 1.00 kg |
203 °F @Load 2.20 lb |
120°C/min; ASTM D1525 |
Kingfa FRABS-518 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmLow temperature impact resistanceApplications:Injection moldingPower tools accessoriesInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Vicat Softening Point | 95.0 °C @Load 5.10 kg |
203 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution PS 147F GPPS Styrolution PS 147F is a highly transparent GPPS grade. It gives excellent mechanical and heat resistance properties while providing with easy processability and short cycle time.Medium FlowEasy pro.. |
|||
Vicat Softening Point | 95.0 °C @Load 5.10 kg |
203 °F @Load 11.2 lb |
ISO 306 |
Borealis MG302Al Polypropylene Compound, Mineral Filled MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt .. |
|||
Vicat Softening Point | 95.0 °C @Load 5.10 kg |
203 °F @Load 11.2 lb |
50°C per hour; ISO 306B50 |
Total Polystyrene Impact 3450 Aesthetic, High Fluidity, High Heat Resistance, High Impact Polystyrene POLYSTYRENE IMPACT 3450 is a high impact polystyrene with high heat resistance, good flow, high stiffness and good aesthetics. With such an ideal balance of properties, POLYSTYRENE IMPACT 3450 is w.. |
|||
Vicat Softening Point | 95.0 °C @Load 5.00 kg |
203 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 1016 V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 95.0 °C @Load 0.999 kg |
203 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 1218 V0/B Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 95.0 °C @Load 5.10 kg |
203 °F @Load 11.2 lb |
120°C/hr; ASTM D 1525 |
Cossa Polimeri ESTALUX 9202 A Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 95.0 °C @Load 5.10 kg |
203 °F @Load 11.2 lb |
120°C/hr; ASTM D 1525 |
Cossa Polimeri ESTALUX 9202 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information.. |
|||
Vicat Softening Point | 95.0 °C @Load 5.10 kg |
203 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Bayblend® FR3000 BBS081 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Impro.. |
|||
Vicat Softening Point | 95.0 °C @Load 5.10 kg |
203 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Bayblend® FR3000 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Easy-.. |
|||
Vicat Softening Point | 95.0 °C @Load 5.00 kg |
203 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Kibilac® PW-957 ASA Polymer Injection |
|||
Vicat Softening Point | 95.0 °C @Load 5.00 kg |
203 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Kibilac® PW-997S ASA Polymer Extrusion |
|||
Vicat Softening Point | 95.0 °C @Load 5.00 kg |
203 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-709 ABS Super impact |
|||
Vicat Softening Point | 95.0 °C @Load 5.00 kg |
203 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-746 ABS - High Flow High flow, medium impact |
|||
Vicat Softening Point | 95.0 °C @Load 5.00 kg |
203 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polyrex® PH-888G Polystyrene - High gloss High impact; high gloss |
|||
Vicat Softening Point | 95.0 °C @Load 0.999 kg |
203 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTASTIR HI 1012 Polystyrene General purpose polystyreneHigh impact resistance, good melt flow rate, good flexibilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 95.0 °C @Load 1.00 kg |
203 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Kibiton® PB-5925 SBC Transparency, high stiffness, injection grade |
|||
Vicat Softening Point | 95.0 °C @Load 5.00 kg |
203 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Polylac® PA-756H ABS - High Flow Super high flow |
|||
Vicat Softening Point | 95.0 °C @Load 5.00 kg |
203 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Polylac® PA-756S ABS - High Flow Super high flow, medium impact |
|||
Vicat Softening Point | 95.0 °C @Load 5.00 kg |
203 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polyrex® PG-33 Polystyrene Standard grade |
|||
Vicat Softening Point | 95.0 °C @Load 5.00 kg |
203 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polyrex® PH-888H Polystyrene - High Impact High FDI; high heat |
|||
Vicat Softening Point | 95.0 °C @Load 1.00 kg |
203 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Wonderloy® PC-510 PC/ABS Alloy - Flame Retardant High Flow |