Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
120°C/min; ASTM D1525 |
Kingfa HF-606 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowModerate UV stabilityHigh stiffnessApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co.,.. |
|||
Vicat Softening Point | 93.0 °C @Load 5.00 kg |
199 °F @Load 11.0 lb |
50°C/min; ASTM D1525 |
Kingfa FRABS V-0 Flame Retardant ABS Features:UL 94 V-0 @ 1.5-3.0mmHigh toughnessFor extrusion moldingApplications:PlateElectric and electronic cabinetPCB boardInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Vicat Softening Point | 93.0 °C @Load 5.10 kg |
199 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution Terlux® HD 2822 MABS Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well .. |
|||
Vicat Softening Point | 93.0 °C @Load 5.00 kg |
199 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 1030 V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, high gloss, good light resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 93.0 °C @Load 5.00 kg |
199 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 1030 V0/Ex Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high impact resistance, high gloss, good light resistance, for extrusionInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 93.0 °C @Load 5.00 kg |
199 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 1030 V0/F Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high melt flow rate, good impact resistance, high gloss, good light resistance, excellent processabilityInformation provided by Co.. |
|||
Vicat Softening Point | 93.0 °C @Load 5.00 kg |
199 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTADIENE 2525 AS Acrylonitrile Butadiene Styrene ABS with high impact resistanceGood melt flow rate, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 93.0 °C @Load 5.10 kg |
199 °F @Load 11.2 lb |
120°C/hr; ISO 306 |
Cossa Polimeri ESTALUX 5513 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 93.0 °C @Load 0.999 kg |
199 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTASTIR GP 1000 Polystyrene Polystyrene crystal, general purposeGood melt flow rate, stiffness, gloss, excellent transparencyInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 93.0 °C @Load 5.10 kg |
199 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® FR3210 TV PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Kibiton® PB-5903 SBC High transparency, high toughness, PS Impact modifier |
|||
Vicat Softening Point | 93.0 °C @Load 5.00 kg |
199 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-737 ABS - High Flow High flow, medium impact |
|||
Vicat Softening Point | 93.0 °C @Load 1.00 kg |
199 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Polyrex® PG-22 Polystyrene TPE compound |
|||
Vicat Softening Point | 93.0 °C @Load 5.00 kg |
199 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polyrex® PH-55Y Polystyrene - Food Medium impact |
|||
Vicat Softening Point | 93.0 °C @Load 5.00 kg |
199 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polyrex® PH-88S Polystyrene - Extrusion Extrusion |