Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 89.0 °C @Load 5.001 kg |
192 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANFILL FOIL ABYX52C1 PP/PE, Thermoforming Grade Information provided by Polykemi AB |
|||
Vicat Softening Point | 89.0 °C @Load 1.02 kg |
192 °F @Load 2.25 lb |
50°C/h; ISO 306 |
Styrolution PS 165 N/L GPPS Styrolution PS 165N/L is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.High molecular weightGood flow characteristicsAppropriate for blending with HIPS.. |
|||
Vicat Softening Point | 89.0 °C @Load 5.10 kg |
192 °F @Load 11.2 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 495N HIPS Styrolution PS 495N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.High flowGood balance of toughness and heat resistanceUL 94 HBInfor.. |
|||
Vicat Softening Point | 89.0 °C @Load 5.10 kg |
192 °F @Load 11.2 lb |
ISO 306 |
Borealis HK030U Polypropylene Compound HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wit.. |
|||
Vicat Softening Point | 89.0 °C @Load 5.10 kg |
192 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPM H350 Polypropylene, Homopolymer Medical Grade Polypropylene PPM H350 is a homopolymer with a Melt Flow Index of 35 g/10 min recommended for the manufacture of medical packaging and medical devices, to the exclusion of implants.Polypropylene PPM.. |
|||
Vicat Softening Point | 89.0 °C @Load 5.00 kg |
192 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTASTIR HI 0412 Polystyrene Polystyrene for injection molding or extrusionHigh impact resistance, good thermal resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 89.0 °C @Load 5.00 kg |
192 °F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
Cossa Polimeri ESTASTIR HI 10 V0 Flame Retardant Polystyrene Flame retardant class V0, with PBDE, for injection molding or extrusionInformation provided by Cossa Polimeri S.r.l. |
|||
Vicat Softening Point | 89.0 °C @Load 1.00 kg |
192 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Kibiton® PB-5910 SBC High transparency, medium stiffness, toughness |
|||
Vicat Softening Point | 89.0 °C @Load 5.00 kg |
192 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polyrex® PH-88 Polystyrene - High Impact High impact |
|||
Vicat Softening Point | 89.0 °C @Load 5.00 kg |
192 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Polyrex® PH-88S Polystyrene - Extrusion Extrusion |
|||
Vicat Softening Point | 89.0 °C @Load 5.00 kg |
192 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Polyrex® PG-33 Polystyrene Standard grade |
|||
Vicat Softening Point | 89.0 °C @Load 5.001 kg |
192 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T5040 FC Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 89.0 °C @Load 5.001 kg |
192 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PPH T5040 FC VT Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |