Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 64.0 °C @Load 5.10 kg |
147 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Styrolution Styrolux S SBC Styrolux S is a new developmental, clear styrene-butadiene copolymer (SBC) designed specifically for blending with Styrolux T in order to enable high performance film extrusion and shrink film appli.. |
|||
Vicat Softening Point | 64.0 °C @Load 5.10 kg |
147 °F @Load 11.2 lb |
ISO 306 |
Borealis BC612WG Polypropylene Copolymer BC612WG is a polypropylene copolymer intended for injection molding. The product is available in natural but other colors can be provided on request. This material has excellent balanced mechanical.. |
|||
Vicat Softening Point | 64.0 °C @Load 5.10 kg |
147 °F @Load 11.2 lb |
ISO 306 |
Borealis Daplen™ EF341AE Polypropylene TPO Compound Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |