Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 43.0 °C @Load 5.10 kg |
109 °F @Load 11.2 lb |
ISO 306 |
Borealis Daplen™ ED117AE Polypropylene TPO Compound Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |