Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 100 - 155 °C @Load 0.999 kg |
212 - 311 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A |
EPICHEM Epicarb PC BLACK IQ Polycarbonate Characteristics: good fluidity, good impact, industrial quality |
|||
Vicat Softening Point | 150 - 155 °C @Load 0.999 kg |
302 - 311 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A |
EPICHEM Epilon PC IX3000 Polycarbonate, High Impact Characteristics: high fluidity, high impact |
|||
Vicat Softening Point | 150 - 155 °C @Load 0.999 kg |
302 - 311 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A |
EPICHEM Epilon PC UVR Polycarbonate, High Impact Characteristics: high fluidity, high impact, UV resistant |
|||
Vicat Softening Point | 150 - 155 °C @Load 0.999 kg |
302 - 311 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A |
EPICHEM Epicarb PC Polycarbonate Characteristics: high fluidity, good impact |