Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 52.0 °C @Load 5.10 kg |
126 °F @Load 11.2 lb |
ISO 306 |
Borealis Daplen™ EE260AI Polypropylene TPO Compound Daplen™ EE260AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |