Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 124 °C @Load 1.00 kg |
255 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYelast TPE 10012 R3 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Vicat Softening Point | 124 °C @Load 5.001 kg |
255 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYlux 104 HF PC/PBT-Blend, High Flow Information provided by Polykemi AB |
|||
Vicat Softening Point | 124 °C @Load 0.999 kg |
255 °F @Load 2.20 lb |
120°C/min; ASTM D1525/A, ISO 306/A |
EPICHEM Epiryl B PPO Polyphenylene oxide |
|||
Vicat Softening Point | 124 °C @Load 1.00 kg |
255 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYabs H00 ABS, Heat Resistant Information provided by Polykemi AB |