Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 138 - 288 °C | 280 - 550 °F | |
Neutrex Purgex™ 456 Plus Purging Compound Blend, polyethylene, and FDA-approved active component. Non-toxic, non-abrasive, and safe. Ready to use and easy to remove.PURGEX 456 Plus is used for color and/or material changes and the removal o.. |
|||
Maximum Service Temperature, Air | 149 - 288 °C | 300 - 550 °F | |
Neutrex Purgex™ 457 Purging Compound Blend, polyethylene, 3% glass, and an FDA-approved active component. Non-toxic, non-abrasive, and safe. Ready to use and easy to removePURGEX 457 Plus is used for color and/or material changes and t.. |
|||
Maximum Service Temperature, Air | 204 - 288 °C | 400 - 550 °F | High Temperature Engineering Plastics |
Claude Bamberger Bamberko® 9016 Purge Compound Bamberko® is recommended for cellulosics, polyolefins, styrenics, and PVC resins. Temperature range 350-525°F (176-275°C). Formulated to flow through injection cylinders and extrusion barrels w.. |