Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 50.0 - 190 °C | 122 - 374 °F | Average value: 120 °C Grade Count:257 |
Overview of materials for PVC, Flexible Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Maximum Service Temperature, Air | 60.0 - 190 °C | 140 - 374 °F | Average value: 167 °C Grade Count:35 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Maximum Service Temperature, Air | 90.0 - 190 °C | 194 - 374 °F | Average value: 110 °C Grade Count:6 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Maximum Service Temperature, Air | 85.0 - 190 °C | 185 - 374 °F | Average value: 147 °C Grade Count:14 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Maximum Service Temperature, Air | 135 - 190 °C | 275 - 374 °F | Average value: 150 °C Grade Count:22 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |