Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 82.2 - 149 °C | 180 - 300 °F | Average value: 104 °C Grade Count:5 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Maximum Service Temperature, Air | 70.0 - 149 °C | 158 - 300 °F | Average value: 99.5 °C Grade Count:57 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |