Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® 1SBVX-30H LDS black PA1010-GF30 Product Description: Grilamid 1SBVX-30H LDS black is a 30% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® AG-25 HM PA66-GF25 Product description: Grilon AG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA66 injection molding grade with 25% glass fibers. Grilon AG-25 HM has the following important pro.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® AG-30 LF 15 PA66-(GF+Z)45 Product description: Grilon AG-30 LF 15 black 9832 is a heat stabilized, normal viscosity PA66 injection molding grade with 30% glass fibers and 15% of a combination of PTFE and silicone. Grilon AG-.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® AZ 3 PA66 Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® AZ 3/2 PA66 Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesE.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® BG-35 S PA6-GF35 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® BZ 1/2 PA6 Product description: Grilon BZ 1/2 is an unreinforced, impact modified PA6 injection molding grade with normal melt viscosity. Grilon BZ 1/2 has the following important properties: Good flow behavio.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® L 16 LM PA12 Product Description: Grilamid L 16 LM is a , low viscosity extrusion type, based on Polyamide 12 (PA12). Grilamid L 16 LM is UV- and heat stabilized. The modification with a nucleation agent results.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® L 20 GM PA12 Product Description: Grilamid L 20 GM is a medium viscosity, heat stabilized polyamide 12 non-reinforced injection molding grade. This product has very good flow characteristics. Special features of.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® L 20 H FR PA12 FR Product Description: Grilamid L 20 H FR is a flame retarded, medium viscosity product, based on Polyamide 12 (PA12). Grilamid L 20 H FR contains no halogen or phosphorus, it has a light natural colo.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® L 20 LF grey PA12 Product Description: Grilamid L 20 LF grey is a medium viscosity graphite filled Polyamide 12 (PA12) grade suitable for both injection molding and extrusion applications. Grilamid L 20 LF grey has b.. |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® L 20 W 20 grey 9280 PA12 Product Description: Grilamid L 20 W 20 grey 9280 is a semiflexible plasticized medium viscosity polyamide 12 (PA12) extrusion grade. Grilamid L 20 W 20 grey 9280 is heat stabilized. The main featur.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® L 20A Z PA12 Product Description: Grilamid L 20A Z is a medium viscosity product, based on Polyamide 12 (PA12). Grilamid L 20A Z is impact modified, hydrolysis-and heat stabilized. Grilamid L 20A Z is used for p.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® L 25 nat 6112 PA12 Product Description: Grilamid L 25 natural 6112 is a high viscous, Polyamide 12 extrusion grade. Grilamid L 25 natural 6112 fulfils the requirements of DIN 73378, Type PA 12-H. Application examples:.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® LM-05 HX nat PA12 Product description: Grilamid LM-05 HX natural is a medium viscosity, heat-stabilized nanocomposite PA12 extrusion and injection molding grade. The special features of Grilamid LM-05 HX natural are:.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® TSG-30/4 FA PA666-GF30 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® TSG-30/4 LF 15 PA666-(GF+Z)45 Product description: Grilon TSG-30/4 LF 15 natural is a normal viscosity, heat stabilized PA 66 + PA 6- molding type with 30% glass fibre reinforcement and 15% of a combination PTFE and siliconoil. .. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® TSG-30/4 LF 15/1 PA666-(GF+Z)45 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® TSS PA666 Product description: Grilon TSS is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS has the following important properties: Excellent flow behaviorHi.. |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® XE 3982 PA12 Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch.. |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® BG-50 HM PA6-GF50 Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop.. |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® BR 40 PA6 Product description: Grilon BR 40 is a medium viscosity, unreinforced, heat stabilized PA6 grade for injection mounding and extrusion applications. Grilon BR 40 has the following important propertie.. |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® L 22A W 40 X PA12-I Product Description: Grilamid L 22A W 40 X is a flexible plasticized and impact modified heat and light stabilized Polyamide 12 (PA12). The main features of Grilamid L 22A W 40 X are: Good impact st.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® L 25 W 40 ESD PA12 Product Description: Grilamid L 25 W 40 ESD is a high viscosity, anti-static highly flexible extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 ESD is plasticized and heat stabilized The inh.. |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® L 25 W 40 HL X PA12-I Product Description: Grilamid L 25 W 40 HLX is a flexible Polyamide 12 grade with an excellent cold impact strength and heat stability. Grilamid L 25 W 40 HLX is specially suitable for flexible tube.. |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® TRV-4X9 PAMACM12-GF40 Product description: Grilamid TRV-4X9 is an amorphous, cycloaliphatic polyamide with 40% glass fibre reinforcement. Grilamid TRV-4X9 characterises itself through the following features: Very low shr.. |
|||
Maximum Service Temperature, Air | 100 - 110 °C | 212 - 230 °F | Heat distortion temperature |
Abatron AboCast 50-3/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Honey viscosity, light amber color. Best combination of high strength and versatility for Abatron "VR" Epoxies. Shelf life is 12+ months.Processin.. |
|||
Maximum Service Temperature, Air | 90.0 - 110 °C | 194 - 230 °F | long term; EMS |
EMS-Grivory Grivory® BM-30/2 PA6-MD30 Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App.. |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® TRVX-50X9 black 9230 PAMACM12-GF50 Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and.. |
|||
Maximum Service Temperature, Air | 80.0 - 110 °C | 176 - 230 °F | long term; EMS |
EMS-Grivory Grivory® TRVX-50X9 nat PAMACM12-GF50 Product description: Grilamid TRVX-50X9 is a 50% glass fiber reinforced amorphous polyamide. This product shows a very low tendency of distortion and is therefore especially suitable for complex and.. |