Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 482 °C | 900 °F | |
Garlock 9850 Compressed Carbon Fiber Gasketing, Nitrile Binder Carbon fibers with a nitrile binder.Carbon fiber gasketing excels in harshest conditions - intense heat, high pressure, saturated steam and hot oils.Laboratory-tested for fire safety.Long-lasting se.. |
|||
Maximum Service Temperature, Air | 482 °C | 900 °F | Short Term |
Mid-Mountain Materials HYTEX® 5000 High Carbon Industrial Textile (PAN) Description: HYTEX is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying chemi.. |
|||
Maximum Service Temperature, Air | 482 °C | 900 °F | Short Term |
Mid-Mountain Materials HYTEX® 5100 High Carbon Industrial Textile (PAN) Description: HYTEX is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying chemi.. |
|||
Maximum Service Temperature, Air | 482 °C | 900 °F | Upper limit of working range |
Heatbath/Park Durastrip 1500 Cleaning Salt An improved low temperature molten salt bath mixture that will rapidly strip all types of paint. The low temperature allows reclaim of scrap parts that can be immediately repainted without further s.. |
|||
Maximum Service Temperature, Air | 482 °C | 900 °F | Upper limit of working range |
Heatbath/Park Durastrip M-3 Cleaning Salt A highly alkaline and oxidizing salt bath mixture that will rapidly strip all types of paint. Enamels, lacquers, varnishes, porcelain enamels and all other types of paint, including hard to strip ep.. |
|||
Maximum Service Temperature, Air | 482 °C | 900 °F | Continuous |
Garlock 9800 Compressed Carbon Fiber Gasketing, SBR Binder Carbon fibers with a SBR binder.Carbon fiber gasketing excels in harshest conditions- intense heat, high pressure, saturated steam and hot oilsLaboratory tested for fire safetyMaintains effective se.. |
|||
Maximum Service Temperature, Air | 482 °C | 900 °F | continuous operation |
3M CG-22 FB-900 Filter Bag 3M has developed a line of advanced textiles for manufacturing high temperature filter bags which can be used at temperatures up to 700°F (371°C), or for those even higher temperature applications.. |
|||
Maximum Service Temperature, Air | 482 °C | 900 °F | |
Aremco Corr-Paint™ CP5000 High Temperature Protective Coating Inorganic, Zinc Filled CP5000 is a two part, water-based, inorganic zinc rich primer which provides superior resistance to salt-fog, immersion, impact and abrasion. This primer system is compatible with all CP-Series prod.. |
|||
Maximum Service Temperature, Air | 482 °C | 900 °F | Stainless |
Aremco HiE-Coat™ 840-CM High Emissivity Coating, Inorganic-Ceramic Filled Ceramic-based, black-pigmented coating for dense refractories to 2500°F (1371°C) and stainless steel to 900°F (482°C) |
|||
Maximum Service Temperature, Air | 482 °C | 900 °F | Continuous |
Aremco Aremco-Seal™ 4030 High Temperature Specialty Coatings Silicone, Ceramic Filled Translucent-white, low-viscosity sealer for porous materials to 900°F (482°C) |
|||
Maximum Service Temperature, Air | 482 °C | 900 °F | Continuous |
Aremco Glass-Coat™ SGC4000 High Temperature Specialty Coatings Silicone-Glass Silicone-glass-ceramic, gray, low viscosity, scratch resistant coating for stainless steel to 900°F (482°C) |
|||
Maximum Service Temperature, Air | 482 °C | 900 °F | |
Aremco Ceramacast™ 905 Silicon-Ceramic Potting Compound Ceramacast™ 905 is a silicone-bonded, ceramic filled high temperature adhesive and potting compound. |